Material Type

Metal

Material Sub-Type

Aluminum

Material Name

Aluminum 7075-T6

Aluminum 7075-T6 is a high-strength alloy that is commonly used in the aerospace and defense industries. It is well-known for its excellent strength-to-weight ratio, making it an ideal material for applications where weight is a critical factor. It is also highly resistant to corrosion, making it well-suited for use in marine environments. In addition, the alloy has good machinability and is easily weldable, making it a versatile option for many manufacturing processes. It is also relatively easy to form and has excellent surface finish capabilities, making it an attractive choice for many applications.

Cost
Lead Time

2-3 Days

Processes

CNC Machining

Metric

English

Note: Properties are not guaranteed. They are intended only as a basis for comparison and not for design purposes.

Last Updated:2 months ago
Mechanical Properties

Yield Tensile Strength

503 MPa

Ultimate Tensile Strength

572 MPa

Tensile Modulus

72 GPa

Shear Strength

331 MPa

Shear Modulus

26 GPa

Fatigue Strength

159 MPa

Elongation At Break

11 %

Poisson's Ratio

0.32

Hardness

B87/150

Density

2.8 g/cm³

Impact Strength (ASTM)

-

Electrical/Magnetic Properties

Surface Resistance (ANSI)

5.0 µΩ

Magnetism

Non-Magnetic

Thermal Properties

Heat Deflection Temperature

-

Thermal Expansion Coefficient

21.6 µm/(m⋅°C

Specific Heat Capacity

0.960 J/g°C

Thermal Conductivity

130 W/(m⋅°C)

Melting Point

447 °C

Chemical Properties

Corrosion Resistance

Moderate

Aluminum 7075-T6

Strong and lightweight aluminum

Get your parts manufactured today.

Get Instant Quote

Material Datasheet

Material Type

Metal

Material Sub-Type

Aluminum

Material Name

Aluminum 7075-T6

Note: Properties are not guaranteed. They are intended only as a basis for comparison and not for design purposes.

Mechanical Properties

Yield Tensile Strength

503 MPa

73.0 Ksi

Ultimate Tensile Strength

572 MPa

83.0 Ksi

Tensile Modulus

72 GPa

10.4 Msi

Shear Strength

331 MPa

48.0 Ksi

Shear Modulus

26 GPa

3.8 Msi

Fatigue Strength

159 MPa

23.0 Ksi

Elongation At Break

11 %

-

Poisson's Ratio

0.32

-

Hardness

B87/150

-

Density

2.8 g/cm³

0.101 lb/in³

Impact Strength (ASTM)

-

-

Electrical/Magnetic Properties

Surface Resistance (ANSI)

5.0 µΩ

-

Magnetism

Non-Magnetic

-

Thermal Properties

Heat Deflection Temperature

-

-

Thermal Expansion Coefficient

21.6 µm/(m⋅°C

12.0 µin/(in⋅°F)

Specific Heat Capacity

0.960 J/g°C

0.229 BTU/lb-°F

Thermal Conductivity

130 W/(m⋅°C)

75.1 BTU/(h⋅ft⋅°F)

Melting Point

447 °C

837 °F

Chemical Properties

Corrosion Resistance

Moderate

-