Material Type

Metal

Material Sub-Type

Other Metals

Material Name

Copper C110

Copper C110, also known as UNS C10100, is a type of oxygen-free copper that is known for its high electrical and thermal conductivity. It is a very pure form of copper, with a minimum conductivity rating of 101% IACS. Copper C110 is commonly used in applications where high electrical conductivity and low electrical resistance are required, such as in the manufacturing of electrical wire and cable. It is also used in the production of corrosion-resistant products, such as pipes and tubes, due to its high resistance to atmospheric corrosion. Copper C110 is generally easy to work with, making it a popular choice among manufacturers.

Cost
Lead Time

2-3 Days

Processes

CNC Machining

Metric

English

Note: Properties are not guaranteed. They are intended only as a basis for comparison and not for design purposes.

Last Updated:2 months ago
Mechanical Properties

Yield Tensile Strength

69 MPa

Ultimate Tensile Strength

221 MPa

Tensile Modulus

117 GPa

Shear Strength

152 MPa

Shear Modulus

43 GPa

Fatigue Strength

97 MPa

Elongation At Break

55 %

Poisson's Ratio

0.34

Hardness

B10/57

Density

8.9 g/cm³

Impact Strength (ASTM)

-

Electrical/Magnetic Properties

Surface Resistance (ANSI)

2.0 µΩ

Magnetism

Non-Magnetic

Thermal Properties

Heat Deflection Temperature

-

Thermal Expansion Coefficient

17.0 µm/(m⋅°C

Specific Heat Capacity

0.385 J/g°C

Thermal Conductivity

388 W/(m⋅°C)

Melting Point

1065 °C

Chemical Properties

Corrosion Resistance

Good

Copper C110

High-purity and electrically conductive copper

Get your parts manufactured today.

Get Instant Quote

Material Datasheet

Material Type

Metal

Material Sub-Type

Other Metals

Material Name

Copper C110

Note: Properties are not guaranteed. They are intended only as a basis for comparison and not for design purposes.

Mechanical Properties

Yield Tensile Strength

69 MPa

10.0 Ksi

Ultimate Tensile Strength

221 MPa

32.0 Ksi

Tensile Modulus

117 GPa

17.0 Msi

Shear Strength

152 MPa

22.0 Ksi

Shear Modulus

43 GPa

6.3 Msi

Fatigue Strength

97 MPa

14.0 Ksi

Elongation At Break

55 %

-

Poisson's Ratio

0.34

-

Hardness

B10/57

-

Density

8.9 g/cm³

0.322 lb/in³

Impact Strength (ASTM)

-

-

Electrical/Magnetic Properties

Surface Resistance (ANSI)

2.0 µΩ

-

Magnetism

Non-Magnetic

-

Thermal Properties

Heat Deflection Temperature

-

-

Thermal Expansion Coefficient

17.0 µm/(m⋅°C

9.4 µin/(in⋅°F)

Specific Heat Capacity

0.385 J/g°C

0.092 BTU/lb-°F

Thermal Conductivity

388 W/(m⋅°C)

224.0 BTU/(h⋅ft⋅°F)

Melting Point

1065 °C

1949 °F

Chemical Properties

Corrosion Resistance

Good

-

www.protoxyz.com